10100 Sour top of the line corrosion in the presence acetic acid

Thursday, March 18, 2010: 11:15 AM
206 A/B (Henry B. Gonzales Convention Center)
Marc Singer*1, Bruce Brown1, Srdjan Nesic1, and Alvaro Camacho2
(1)Ohio University; (2)Lloyd's Register TS
Under stratified flow and dewing conditions, internal corrosion can occur at the top of horizontal pipelines where continuous injection of corrosion inhibitors does not have a mitigating effect. This research work presents an experimental study of the influence of the presence of H2S (up to 0.13 bars) and acetic acid (up to 1000 ppm) on the more standard CO2 Top of the Line Corrosion. A comprehensive analysis on the effect of these parameters on the type of corrosion product film formed at the top of the line is performed as well.