High-Temperature Issues and Materials for the Process Industry - TEG 123X/TEG 126X/TEG 128X/TEG 270X

Tuesday, March 15, 2011: 7:55 AM-5:00 PM
Room 320 B (George R. Brown Convention Center)
Chair:
Roman Pankiw
Vice Chair:
Vilupanur A. Ravi
8:00 AM
8:50 AM
An Approach to Determine the Initiation of Carburization in a 304H Stainless Steel Piping under Petrochemical Environment
Jeffrey Xie*1, Marek Crawford1, Lorrie Davies2, David Eisenhawer2, Randy Saunders2, and Les Benum2
(1)NOVA Chmicals Corporation; (2)NOVA Chemicals Corporation
9:15 AM
9:30 AM
Life Assessment of Reformer Tubes from Strain Measurement
Charles W. Thomas*, Ted L. Anderson, and Tim Hill
Quest Integrity Group
9:55 AM
Creep Failure by Steam Oxidation Scale of 9Cr Boiler Tubes After Long-Time Service
Hiroyasu Matsuda*1, Masahiko Takehara2, Koji Kawano3, Shigemitsu Kihara4, Kouichi Yagi5, and Daisuke Horikoshi6
(1)Mitsui Chemicals,INC., Engineering Div, Production & Technology Center; (2)Idemitsu Kosan Co,Ltd. ,Plant Management & Technology Center, Manufacturing Department; (3)Idemitsu Engineering Co., Ltd.; (4)Best Materia Co.,Ltd; (5)Material Consultant; (6)Maruzen Petrochemical Co., LTD./Production Administration Dept.
10:45 AM
Metal Dusting: Kinetically or Thermodynamically Controlled?
Chrétien Hermse*
TNO Science and Industry
11:10 AM
1:00 PM
Damaged Long Seam Weld on an Outlet Elbow outside Hotbox of an Ethane Cracking Furnace
Jeffrey Xie*1, Marek Crawford1, David Eisenhawer2, Chris Sturdy2, Mark Maxwell2, Lorrie Davies2, and Les Benum2
(1)NOVA Chmicals Corporation; (2)NOVA Chemicals Corporation
1:25 PM
2:40 PM
2:55 PM
The Influence of Surface Pre-Treatment on the Metal Dusting Behavior of Cast and Wrought 20Cr32NiFe
Chrétien Hermse*1, Henrik Asteman2, R. M. IJzerman1, and Dietlinde Jakobi2
(1)TNO Science and Industry; (2)Schmidt + Clemens GmbH + Co. KG
3:20 PM
Chromizing of 3-Cr Steel
Vilupanur Ravi*1, Bradley Harrison1, Jordan Koch1, Alexander L. Ly2, Andrew Schissler1, Bruce A. Pint3, and James Allen Haynes3
(1)Cal Poly Pomona; (2)California Polytechnic University, Pomona; (3)Oak Ridge National Lab
3:45 PM
A New Lean Nickel Alloy for Use in High Temperature Industrial and Automotive Applications
Larry D. Paul*1 and Heike Hattendorf2
(1)Thyssen Krupp VDM USA Inc; (2)ThyssenKrupp VDM
4:10 PM
Corrosion Behavior of High Chromium White Irons in High Temperature Caustic
Richard E. Clegg* and Alan J. McLeod
Process Engineering and Light Metals Centre, CQUniversity Australia
4:35 PM
A Prominent Ni-Cr-Si-Cu Alloy Resisting in Metal Dusting
Yoshitaka Nishiyama1, Hirokazu Okada1, Takahiro Osuki1, Shinnosuke Kurihara2, and Satoshi Matsumoto*3
(1)Sumitomo Metal Industries, Ltd. Corporate Research and Development Laboratories; (2)Sumitomo Metal Industries, Ltd. Steel Tube Works; (3)Sumitomo Metal USA, Inc.
See more of: Technical Symposium